Characterization of hydroxyapatite by electron microscopy.
???displayArticle.abstract???
The obtention of hydroxyapatite (HAp) is reported using brushite (CaHPO4.2H2O) and the skeleton of a starfish (Mellita eduardobarrosoi sp. nov.), primarily composed of magnesian calcite ((Ca,Mg)CO3) as precursors. Stoichiometric amounts of both were reacted under hydrothermal conditions: a pressure of 5.8 MPa and a temperature of 200 degrees C for 2, 4, 6, 8, 10, and 20 h of reaction times. The samples obtained were characterized by means of scanning electron microscopy, X-ray diffraction, infrared spectroscopy, and transmission electron microscopy. Two defined populations of HAp fibers were found: A bundle of fibers 75 mum in length and 1-13 mum in diameter, and a second bundle of fibers 5 mum in length and less than 0.5 mum in diameter. Furthermore, an increase in HAp formation and a Ca/P ratio as a function of reaction time were observed. The growth mechanism of HAp is also discussed.
???displayArticle.pubmedLink??? 17481330
???displayArticle.link??? Microsc Microanal